膩?zhàn)臃勖摲??原來是這些原因?qū)е碌模?/p>
來源:http://www.cqokncn.cn 日期:2025-08-18 發(fā)布人:
膩?zhàn)邮且环N用于墻面修補(bǔ)的基材,為接下來的裝修(繪畫、壁紙)打下良好的基礎(chǔ)。膩?zhàn)臃譃閮?nèi)墻和外墻,外墻膩?zhàn)涌癸L(fēng)、耐曬,附著性高,強(qiáng)度高,環(huán)保指標(biāo)略低。
Putty is a substrate used for wall repair, laying a good foundation for subsequent decoration (painting, wallpaper). Putty is divided into interior and exterior walls. Exterior wall putty is wind resistant, sun resistant, has high adhesion, high strength, and slightly lower environmental indicators.
膩?zhàn)臃?/p>
Putty powder
有部分人反饋,現(xiàn)在膩?zhàn)臃勖摲蹖?dǎo)致乳膠漆脫落、鼓包開裂是一個(gè)較為嚴(yán)重的問題。目前膩?zhàn)幼畛R姷墓ず髥栴}是膩?zhàn)臃鄣舴?、掉白?/p>
Some people have given feedback that the detachment of putty powder causing latex paint to peel off, bulge and crack is a serious problem. The most common post work problem with putty at present is the loss of putty powder and whitening.
1.粘合強(qiáng)度不夠,導(dǎo)致脫粉。廠家盲目降低成本,膠粉的粘結(jié)強(qiáng)度差,添加量少,尤其是對(duì)于膩?zhàn)觾?nèi)墻而言,粘結(jié)強(qiáng)度與膠粉和膠水的質(zhì)量和添加量密切相關(guān)。
1. Insufficient adhesive strength leads to powdering. Manufacturers blindly reduce costs, resulting in poor bonding strength and low dosage of adhesive powder, especially for putty interior walls. The bonding strength is closely related to the quality and dosage of adhesive powder and glue.
2.在使用膩?zhàn)訒r(shí),膩?zhàn)拥牟牧线x擇和結(jié)構(gòu)非常重要,但它對(duì)諸如雙飛粉、滑爽石粉,硅粉石粉等填料沒有影響。但是,羧甲基纖維素鈉不能用作防水膩?zhàn)雍屯鈮δ佔(zhàn)樱驗(yàn)轸燃谆w維素鈉與石灰鈣粉和白水泥漿反應(yīng),會(huì)導(dǎo)致脫粉。此外,在石灰鈣粉和白水泥漿中加入聚丙烯酰胺作為防水涂料也會(huì)因化學(xué)反應(yīng)而脫粉。
When using putty, the material selection and structure of putty are very important, but it has no effect on fillers such as double fly powder, smooth stone powder, silica powder, etc. However, sodium carboxymethyl cellulose cannot be used as waterproof putty and exterior wall putty because it reacts with lime calcium powder and white cement slurry, causing powdering. In addition, adding polyacrylamide as a waterproof coating to lime calcium powder and white cement slurry can also cause powdering due to chemical reactions.
3.混合攪拌不均勻是脫粉的主要原因,國(guó)內(nèi)有些廠家生產(chǎn)膩?zhàn)臃鄣脑O(shè)備簡(jiǎn)單,不是專用的攪拌設(shè)備,混合不均勻?qū)е履佔(zhàn)用摲邸?/p>
3. Uneven mixing is the main reason for powder removal. Some domestic manufacturers have simple equipment for producing putty powder, which is not a dedicated mixing equipment. Uneven mixing leads to powder removal of putty.
以上的內(nèi)容來自:濟(jì)南石膏粉更多的精彩內(nèi)容請(qǐng)點(diǎn)擊我們的網(wǎng)站:http://www.cqokncn.cn
The above content comes from: Jinan gypsum powder. For more exciting content, please click on our website: http://www.cqokncn.cn